Exposed aggregate is one of the most popular driveway finishes in Brisbane, and one of the most commonly damaged by the wrong kind of cleaning. Because the surface is made of stones held in place by a thin layer of cement, it needs a different approach from plain concrete. This guide covers how to clean exposed aggregate properly, how to deal with sealer that has gone patchy or white, and how to reseal it so it lasts.

What makes exposed aggregate different

Exposed aggregate is made by washing back the top layer of fresh concrete to reveal the stones underneath. What holds those stones in place is the cement paste around them. That paste is the weak point. Too much pressure, a narrow nozzle held too close, or harsh acid cleaning can erode the paste and loosen stones, leaving small pits and a rough, gappy surface.

That is why exposed aggregate should be cleaned with a rotary surface cleaner at an appropriate pressure, not with a pencil jet.

Common problems with exposed aggregate

  • Dull, grey stones. The aggregate has lost its colour because the old sealer has worn off, or a layer of dirt is covering it.
  • Black and green growth between the stones. Mould and algae grow in the small gaps, especially on shaded driveways.
  • White or cloudy sealer. Moisture has got trapped under an acrylic sealer, or the sealer was applied too thickly or onto damp concrete.
  • Peeling sealer. The old coat has lost its grip, usually in the wheel tracks.
  • Oil and rust stains. These soak into the paste between the stones.

How we clean exposed aggregate

  1. Pre-treat. Mould and algae are treated first so they are killed, not just knocked back. Oil spots get a degreaser.
  2. Surface clean. A rotary surface cleaner lifts dirt evenly across the whole driveway, without the stripes you get from a hand wand, and without blasting the paste out.
  3. Detail. Edges, joints and the junction with the road kerb and garage are done by hand.
  4. Rinse and check. We check for loose stones, cracking and old sealer before talking about sealing.

For stubborn oil, see how to remove oil stains from a concrete driveway. The same principles apply on aggregate.

Fixing white or cloudy sealer

A white haze in acrylic sealer is very common in Brisbane, because of the humidity and summer storms. In many cases it can be fixed without stripping the whole driveway. Depending on the sealer, it can sometimes be reactivated so the trapped moisture escapes and the sealer clears. If the sealer is too far gone, or is peeling, it has to be stripped back before resealing. Sealing over a failed coat just traps the problem.

Resealing exposed aggregate

Most exposed aggregate in Brisbane is sealed with a solvent-based acrylic, in satin or gloss, which brings the colour of the stones back up and gives the “wet look” many people want. Some points matter a lot:

  • The concrete must be completely dry. Sealing damp aggregate is the main cause of cloudy sealer later.
  • Two thin coats beat one thick one. Thick coats are more likely to trap moisture and turn white.
  • Add anti-slip on slopes. Gloss sealer on a sloping driveway can be slippery when wet, so an anti-slip additive is worth considering.
  • Keep cars off until it has cured. Hot tyres on soft sealer leave marks.

Not sure whether you want a clear or tinted finish? See clear seal vs colour seal. For how long sealers last and what affects the cost, see concrete sealing: cost factors and lifespan.

How often to reseal exposed aggregate

An acrylic-sealed exposed aggregate driveway usually needs a maintenance coat every few years, sooner if it is in full sun or gets heavy car traffic. The sign to watch for is water soaking in rather than beading, and the stones looking dull in the wheel tracks. Topping up before the sealer wears through is quicker and cheaper than stripping and starting again.

Frequently asked questions

Can pressure cleaning damage exposed aggregate?

Yes, if it is done wrong. Too much pressure or a narrow jet can erode the cement between the stones and loosen them. A surface cleaner at the right pressure cleans it safely.

Why has my sealed aggregate driveway gone white?

Usually trapped moisture under an acrylic sealer, often from sealing when the concrete was not fully dry or applying it too thickly. It can often be fixed without a full strip.

Should I seal my exposed aggregate driveway?

Most owners do, because sealer brings back the colour of the stones and slows down staining and mould. It does need maintaining every few years.

How long does it take to clean and seal a driveway?

Cleaning is usually done in a few hours. Sealing needs dry concrete, so it is often done on a later dry day, then cars need to stay off while it cures.